Chloride-Induced Stress Corrosion Cracking of Oxide-Dispersion-Strengthened Austenitic Steels
Yan, Xueliang, Wang, Fei, Jiang, Lejun, Qiu, Xiaoxing, Lu, Yongfeng, Nastasi, Michael, Zhou, Zhangjian, Cui, BaiVolume: