![](/img/cover-not-exists.png)
A study on stress corrosion cracking and hydrogen embrittlement of Jethete M152 martensitic stainless steel
Shen, Sicong, Song, Xiaolong, Li, Qizhen, Li, Xinfeng, Zhu, Ruihua, Yang, GongxianVolume:
740-741
Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2018.10.091
Date:
January, 2019
File:
PDF, 5.70 MB
english, 2019