![](/img/cover-not-exists.png)
Dynamic strain aging, deformation and fracture behaviour of the nickel base superalloy Inconel 617
Rao, Ch. Visweswara, Srinivas, N.C. Santhi, Sastry, G.V.S., Singh, VakilVolume:
742
Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2018.10.123
Date:
January, 2019
File:
PDF, 3.57 MB
english, 2019