![](/img/cover-not-exists.png)
Ultrasonic Inspection of a 9% Ni Steel Joint Welded with Ni-based Superalloy 625: Simulation and Experimentation
Payão Filho, João, Passos, Elisa, Gonzaga, Rodrigo, Ferreira, Ramon, Santos, Daniel, Juliano, DiegoVolume:
8
Language:
english
Journal:
Metals
DOI:
10.3390/met8100787
Date:
October, 2018
File:
PDF, 7.05 MB