![](/img/cover-not-exists.png)
Galvanic corrosion in marine environments: Effects associated with the inversion of polarity of Zn/carbon steel couples
Refait, Philippe, Jeannin, Marc, François, Emilie, Sabot, René, Grolleau, Anne-MarieLanguage:
english
Journal:
Materials and Corrosion
DOI:
10.1002/maco.201810568
Date:
November, 2018
File:
PDF, 3.06 MB
english, 2018