![](/img/cover-not-exists.png)
The fractography analysis of IN718 alloy after three-point flexure fatigue test
Belan, Juraj, Vaško, Alan, Kuchariková, Lenka, Tillová, Eva, Vasko, M., Handrik, M., Jakubovičová, L., Kopas, P., Blatnická, M., Baniari, V., Štalmach, O., Sapietová, A., Sága, M.Volume:
157
Year:
2018
Language:
english
Journal:
MATEC Web of Conferences
DOI:
10.1051/matecconf/201815707001
File:
PDF, 1.04 MB
english, 2018