Inhibition Effect of N, N'-Dimethylaminoethanol on the Pitting Corrosion Austenitic Stainless Steel Type 304
LOTO, Roland Tolulope, LOTO, Cleophas Akintoye, POPOOLA, Patricia Abimbola, FEDOTOVA, TatianaVolume:
21
Language:
english
Journal:
Materials Science
DOI:
10.5755/j01.ms.21.4.8977
Date:
November, 2015
File:
PDF, 382 KB
english, 2015