![](/img/cover-not-exists.png)
Inhibition of Pitting Corrosion of the Stainless Steel by Dipyridinium Salts
Obaid, A.Y., Al-Thabaiti, S.A., Qusti, A.H., Hermas, A.A.Volume:
25
Year:
2013
Language:
english
Journal:
Asian Journal of Chemistry
DOI:
10.14233/ajchem.2013.13762
File:
PDF, 1.07 MB
english, 2013