Artificial intelligence to predict inhibition performance of pitting corrosion
Boukhari, Y., Boucherit, M.N, Zaabat, M., Amzert, S., Brahimi, K.Volume:
9
Language:
english
Journal:
Journal of Fundamental and Applied Sciences
DOI:
10.4314/jfas.v9i1.19
Date:
February, 2017
File:
PDF, 1.73 MB