Effect of CCBP doping on the multifunctional Al-0.5 Mg-15CCBP superalloy using liquid metallurgy process for advanced application
Fayomi, O.S.I., Joseph, O.O., Akande, I.G., Ohiri, C.K., Enechi, K.O., Udoye, N.E.Language:
english
Journal:
Journal of Alloys and Compounds
DOI:
10.1016/j.jallcom.2018.12.312
Date:
December, 2018
File:
PDF, 808 KB