![](/img/cover-not-exists.png)
Production and Analysis of Recycled Ammonium Perrhenate from CMSX-4 superalloys
Gonzalez-Rodriguez, J., Pepper, Katherine, Baron, M.G., Mamo, S.K., Simons, A.M.Volume:
16
Journal:
Open Chemistry
DOI:
10.1515/chem-2018-0136
File:
PDF, 493 KB