![](/img/cover-not-exists.png)
Application of time–temperature–humidity superposition to the mass loss of wood through hygrothermally accelerated ageing at 95–140 °C and different relative humidity levels
Zeniya, Nanami, Obataya, Eiichi, Endo-Ujiie, Kaoru, Matsuo-Ueda, MiyukiVolume:
1
Language:
english
Journal:
SN Applied Sciences
DOI:
10.1007/s42452-018-0009-8
Date:
January, 2019
File:
PDF, 1.20 MB
english, 2019