![](/img/cover-not-exists.png)
High temperature tensile behavior of a thin-walled Ni based single-crystal superalloy with cooling hole: In-situ experiment and finite element calculation
Shang, Yong, Zhang, Heng, Hou, Haozhang, Ru, Yi, Pei, Yanling, Li, Shusuo, Gong, Shengkai, Xu, HuibinVolume:
782
Language:
english
Journal:
Journal of Alloys and Compounds
DOI:
10.1016/j.jallcom.2018.12.232
Date:
April, 2019
File:
PDF, 5.25 MB
english, 2019