Nonlinearity from stress corrosion cracking as a function of chloride exposure time using the time reversed elastic nonlinearity diagnostic
Young, Sarah M., Anderson, Brian E., Hogg, Stephen M., Le Bas, Pierre-Yves, Remillieux, Marcel C.Volume:
145
Journal:
The Journal of the Acoustical Society of America
DOI:
10.1121/1.5087828
Date:
January, 2019
File:
PDF, 4.26 MB
2019