![](/img/cover-not-exists.png)
Cutting Performance of CBN Tools in Machining of Nickel Based Superalloy.
SHINTANI, Kazuhiro, KATO, Hideharu, MAEDA, Takao, FUJIMURA, Yoshio, YAMAMOTO, AkiraVolume:
58
Year:
1992
Journal:
Journal of the Japan Society for Precision Engineering
DOI:
10.2493/jjspe.58.1685
File:
PDF, 9.94 MB
1992