Degree of Undercooling and Contact Angle of Pure Iron at 1933 K on Single-crystal Al2O3, MgO, and MgAl2O4 under Argon Atmosphere with Controlled Oxygen Partial Pressure
Shibata, Hiroyuki, Watanabe, Yusuke, Nakajima, Keiji, Kitamura, Shin-yaVolume:
49
Year:
2009
Journal:
ISIJ International
DOI:
10.2355/isijinternational.49.985
File:
PDF, 1.82 MB
2009