Influence of thermal shock behavior on microstructure and mechanical properties of IN718 superalloy
Wang, Shu-liang, Sun, Yan-rong, Du, Li-jing, Liu, Li, Wang, Jie, Xiang, Ding-hanVolume:
484
Journal:
Applied Surface Science
DOI:
10.1016/j.apsusc.2019.04.047
Date:
August, 2019