Self-healing behavior of Inconel 617B superalloy
Kang, Seok-Hyeon, Lee, Sukjin, Suh, Jin-Yoo, Kim, Han-Jin, Lee, Young-KookLanguage:
english
Journal:
Journal of Alloys and Compounds
DOI:
10.1016/j.jallcom.2019.07.204
Date:
July, 2019