Thermal, Nanoindentation and Dielectric Study of Nanocomposites Based on Poly(Propylene Furanoate) and Various Inclusions
Klonos, Panagiotis A., Papadopoulos, Lazaros, Tzetzis, Dimitrios, Kyritsis, Apostolos, Papageorgiou, George Z., Bikiaris, Dimitrios N.Language: