Consideration of recrystallization modeling of γ/γ’-strengthened Ni-based superalloys at sub-solvus temperatures
Nishimoto, Takashi, Okajima, Takuma, Zhang, Qiaofu, Gong, Jiadong, Olson, GregVolume:
1270
Language:
english
Journal:
Journal of Physics: Conference Series
DOI:
10.1088/1742-6596/1270/1/012051
Date:
August, 2019