![](/img/cover-not-exists.png)
Characterization of Fine Metallic Soap Particles by X-Ray Diffraction, Differential Scanning Calorimetry, and Specific Surface Area Analysis
SAWADA, Kouhei, KONAKA, MikiVolume:
53
Year:
2004
Language:
english
Journal:
Journal of Oleo Science
DOI:
10.5650/jos.53.627
File:
PDF, 365 KB
english, 2004