![](/img/cover-not-exists.png)
Preventive Maintenance against Stress Corrosion Cracking in Nuclear Power Reactors by Laser Peening
MUKAI, Naruhiko, SANO, Yuji, YODA, Masaki, CHIDA, Itaru, UEHARA, Takuya, YAMAMOTO, TetsuoVolume:
33
Year:
2005
Language:
english
Journal:
The Review of Laser Engineering
DOI:
10.2184/lsj.33.444
File:
PDF, 4.72 MB
english, 2005