![](/img/cover-not-exists.png)
Investigation of hot corrosion resistance of bare and Ni-20%Cr coated superalloy 825 to Na2SO4-60%V2O5 environment at 900°C
Muthu, S.M., Arivarasu, M., Arivazhagan, N., rao, M.NageswaraVolume:
14
Year:
2019
Language:
english
Journal:
Procedia Structural Integrity
DOI:
10.1016/j.prostr.2019.05.037
File:
PDF, 4.66 MB