Machining behavior of additively manufactured and cast-wrought nickel-based superalloy (IN 625)
Ananda-Kumar, Rajesh Kumar, Moscoso-Kingsley, Wilfredo, Jacob, Gregor, Donmez, Alkan, Madhavan, ViswanathanVolume:
26
Year:
2018
Language:
english
Journal:
Procedia Manufacturing
DOI:
10.1016/j.promfg.2018.07.070
File:
PDF, 1.08 MB
english, 2018