![](/img/cover-not-exists.png)
Molecular Dynamics Based Modelling of Tensile Deformation and Nanoindentation of Tungsten Nanoparticles for Estimating Useful Mechanical Properties
Bandyopadhyay, Krishnan, Ghosh, K.S., Ghosh, M.M.Volume:
5
Year:
2018
Language:
english
Journal:
Materials Today: Proceedings
DOI:
10.1016/j.matpr.2018.06.453
File:
PDF, 604 KB