Atomic force microscopy nano-indentation for testing mechanical properties in thin films
Roa, Simón, Haberkorn, N., Sirena, MartínVolume:
14
Year:
2019
Journal:
Materials Today: Proceedings
DOI:
10.1016/j.matpr.2019.05.065
File:
PDF, 513 KB
2019