Electron force-induced dislocations annihilation and regeneration of a superalloy through electrical in-situ transmission electron microscopy observations
Zhang, Xin, Li, Hongwei, Zhan, Mei, Zheng, Zebang, Gao, Jia, Shao, GuangdaLanguage:
english
Journal:
Journal of Materials Science & Technology
DOI:
10.1016/j.jmst.2019.08.008
Date:
August, 2019