![](/img/cover-not-exists.png)
In Situ Creep Behavior Characterization of Single Crystal Superalloy by UV-DIC at 980 °C
Shang, Yong, Dong, Yali, Pei, Yanling, Ma, Chaoli, Li, Shusuo, Gong, ShengkaiVolume:
9
Journal:
Coatings
DOI:
10.3390/coatings9100598
Date:
September, 2019
File:
PDF, 5.68 MB
2019