Growth of ZnO:Al by atomic layer deposition: Deconvoluting the contribution of hydrogen interstitials and crystallographic texture on the conductivity
Mauit, Ozhet, Caffrey, David, Ainabayev, Ardak, Kaisha, Aitkazy, Toktarbaiuly, Olzat, Sugurbekov, Yerzhigit, Sugurbekova, Gulnar, Shvets, Igor V., Fleischer, KarstenVolume:
690
Journal:
Thin Solid Films
DOI:
10.1016/j.tsf.2019.137533
Date:
November, 2019