The effect of post-irradiation annealing on the stress corrosion crack growth rate of neutron-irradiated 304L stainless steel in boiling water reactor environment
Kuang, Wenjun, Hesterberg, Justin, Was, Gary S.Language:
english
Journal:
Corrosion Science
DOI:
10.1016/j.corsci.2019.108183