![](/img/cover-not-exists.png)
Influence of hydrogen on stress corrosion cracking behavior in Al–10Mg alloy; Al–10Mg合金における応力腐食割れ挙動に及ぼす水素の影響;
Hirayama, Kyosuke, Toda, Hiroyuki, Shimizu, Kazuyuki, Uesugi, Kentaro, Takeuchi, Akihisa, Masunaga, RyoheiVolume:
69
Journal:
Journal of Japan Institute of Light Metals
DOI:
10.2464/jilm.69.223
Date:
April, 2019
File:
PDF, 1.28 MB
2019