![](/img/cover-not-exists.png)
Electrochemical noise generated during the stress corrosion cracking of sensitized alloy 690
J.G. Gonzalez-Rodriguez, M. Casales, V.M. Salinas-Bravo, M.A. Espinosa-Medina, A. Martinez-VillafañeVolume:
8
Language:
english
Pages:
6
DOI:
10.1007/s10008-003-0450-4
Date:
April, 2004
File:
PDF, 359 KB
english, 2004