![](/img/cover-not-exists.png)
Through-Thickness Strain Gradient in a Hot-Rolled Al-Mg Alloy Obtained by Nanoindentation and Glancing Angle X-Ray Diffraction
Parvinian, Sepideh, Hoar, Eric, Tavakoli, David, Shafiei, Mehdi, Garmestani, HamidLanguage:
english
Journal:
Journal of Materials Engineering and Performance
DOI:
10.1007/s11665-019-04400-9
Date:
October, 2019
File:
PDF, 1.10 MB
english, 2019