![](/img/cover-not-exists.png)
Epitaxial laser deposition of single crystal Ni-based superalloy: Variation of stray grains
Chen, Hao, Huang, Guosheng, Lu, Yuanyuan, Lin, Shougang, Liu, DejianVolume:
158
Language:
english
Journal:
Materials Characterization
DOI:
10.1016/j.matchar.2019.109982
Date:
December, 2019
File:
PDF, 2.38 MB
english, 2019