The influence of defects at the steel/concrete interface...

The influence of defects at the steel/concrete interface for chloride-induced pitting corrosion of naturally-deteriorated 20-years-old specimens studied through X-ray Computed Tomography

Rossi, Emanuele, Polder, Rob, Copuroglu, Oguzhan, Nijland, Timo, Šavija, Branko