![](/img/cover-not-exists.png)
Coupling effect of microstructure and hydrogen absorbed during service on pitting corrosion of 321 austenitic stainless steel weld joints
Cao, Ruohan, Xu, Lining, Jiang, Baolong, Gao, Mengjie, Qu, Dingrong, Shan, Guangbin, Xu, Shujian, Qiao, Lijie, Qiao, LijieLanguage:
english
Journal:
Corrosion Science
DOI:
10.1016/j.corsci.2019.108339
Date:
November, 2019
File:
PDF, 3.75 MB
english, 2019