![](/img/cover-not-exists.png)
8th International Symposium on Superalloy 718 and Derivatives (Ott/8th International) || Formation of Nanocrystalline Structure Upon Severe Thermomechanical Processing and its Effect on the Superplastic Properties of Nickel Base Alloys
Ott, Eric, Banik, Anthony, Andersson, Joel, Dempster, Ian, Gabb, Tim, Groh, Jon, Heck, Karl, Helmink, Randy, Liu, Xingbo, Wusatowska-Sarnek, AgnieszkaVolume:
10.1002/97
Year:
2014
Language:
english
DOI:
10.1002/9781119016854.ch57
File:
PDF, 1.33 MB
english, 2014