![](/img/cover-not-exists.png)
Stress Corrosion Cracking of Basalt/Epoxy Composites under Bending Loading
Mahmood M. Shokrieh, Mahdi MemarVolume:
17
Language:
english
Pages:
15
DOI:
10.1007/s10443-009-9116-4
Date:
April, 2010
File:
PDF, 510 KB
english, 2010