High Temperature Tensile Behavior of a Nickel-Based Superalloy 55Ni-17Cr-12Fe-9Mo-2Nb-1.5Al Used in Launch Vehicle Applications
Manikandan, P., Sudarshan Rao, G., Saravanan, K., Chakravadhanula, V. S. K., Amruth, M., Narayana Murty, S. V. S., Sharma, V. M. J., Ramesh Narayanan, P.Language:
english
Journal:
Journal of Materials Engineering and Performance
DOI:
10.1007/s11665-019-04525-x
Date:
December, 2019