![](/img/cover-not-exists.png)
Effect of brass composition and phases on stress corrosion mitigation by laser shock peening
Lisenko, Nikita, Evans, Connor D., Yao, Y. LawrenceVolume:
23
Journal:
Manufacturing Letters
DOI:
10.1016/j.mfglet.2019.11.003
Date:
January, 2020
File:
PDF, 2.55 MB
2020