![](/img/cover-not-exists.png)
Effect of Slag Composition on the Deoxidation and Desulfurization of Inconel 718 Superalloy by ESR Type Slag Without Deoxidizer Addition
Duan, Sheng-Chao, Shi, Xiao, Zhang, Man-Cang, Li, Bin, Yang, Wen-Sheng, Wang, Fei, Guo, Han-Jie, Guo, JingJournal:
Metallurgical and Materials Transactions B
DOI:
10.1007/s11663-019-01729-3
Date:
November, 2019
File:
PDF, 1.66 MB
2019