![](/img/cover-not-exists.png)
Microstructure and mechanical properties of dissimilar nickel-based superalloys resistance spot welds
Bemani, M., Pouranvari, M.Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2019.138825
Date:
December, 2019
File:
PDF, 4.26 MB
2019