Understanding the Interdependence of Penetration Depth and Deformation on Nanoindentation of Nanoporous Silver
Champion, Yannick, Laurent-Brocq, Mathilde, Lhuissier, Pierre, Charlot, Frédéric, Moreira Jorge Junior, Alberto, Barsuk, DariaVolume:
9
Journal:
Metals
DOI:
10.3390/met9121346
Date:
December, 2019