![](/img/cover-not-exists.png)
As-cast microstructure and solidification behavior of a high Al- and Nb-containing superalloy
Lianxu Yu, Yating Zhao, Shulin Yang, Wenru Sun, Shouren Guo, Xiaofeng Sun, Zhuangqi HuVolume:
45
Language:
english
Pages:
9
DOI:
10.1007/s10853-010-4372-0
Date:
July, 2010
File:
PDF, 894 KB
english, 2010