![](/img/cover-not-exists.png)
Microstructure and microhardness of dissimilar weldment of Ni-based superalloys IN718-IN713LC
Ye, R.R., Li, H.Y., Ding, R.G., Doel, T.J.A., Bray, S., Walpole, A., Bowen, P.Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2019.138894
Date:
January, 2020
File:
PDF, 5.44 MB
english, 2020