Atomic layer deposition of Al2O3 on organic potassium terephthalate with enhanced K-storage behavior for K-ion batteries
Deng, Qijiu, Tian, Congcong, Luo, ZongbinJournal:
Ionics
DOI:
10.1007/s11581-019-03434-2
Date:
January, 2020