![](/img/cover-not-exists.png)
Nanoindentation of polymers
Umut D. Cakmak, Thomas Schöberl, Zoltan MajorVolume:
47
Language:
english
Pages:
12
DOI:
10.1007/s11012-011-9481-6
Date:
March, 2012
File:
PDF, 938 KB
english, 2012