![](/img/cover-not-exists.png)
Fractographic analysis of the overload effect on fatigue crack growth in 2024-T3 and 7075-T6 Al alloys
Albedah, A., Bouiadjra, B. Bachir, Mohammed, S. M. A. K., Benyahia, F.Volume:
27
Language:
english
Journal:
International Journal of Minerals, Metallurgy and Materials
DOI:
10.1007/s12613-019-1896-4
Date:
January, 2020
File:
PDF, 1.01 MB
english, 2020