![](/img/cover-not-exists.png)
Analysis of high aspect ratio small holes in rapid electrical discharge machining of superalloys using Taguchi and TOPSIS
Rajamanickam, S., Prasanna, J., Chandrasekhara Sastry, C.Volume:
42
Language:
english
Journal:
Journal of the Brazilian Society of Mechanical Sciences and Engineering
DOI:
10.1007/s40430-020-2180-2
Date:
February, 2020
File:
PDF, 3.62 MB
english, 2020