Microstructure and Mechanical Performance of Graphene Nanosheets Reinforced Nickel-Based Superalloy FGH95 Composite
Gao, Yuxi, Zou, Jinwen, Wang, Xuqing, Wang, Xiaofeng, Yang, Jie, Wang, HuamingVolume:
10
Journal:
Nanomaterials
DOI:
10.3390/nano10010100
Date:
January, 2020
File:
PDF, 4.73 MB